Page 7 - HAMMER HEAT-SHIELD
P. 7

HAMMER HEAT-SHIELD                                          HAMMER HEAT-SHIELD










 Plywood & Laminate surfaces should be free of dust, wax and           Once the tack is formed & the film turns transparent, paste

 stickers. Preferably the surfaces to be glued, should be sanded       the  surfaces  properly.  Bring  the  laminate  in  contact  to

 and cleaned with cloth.                                               HAMMER  HEAT-SHIELD  coated  ply  surface  and  make
                                                                       proper alignment.











 Stir the contents of the glue container just before application

 &  spread  the  glue  uniformly  with  a  plastic  notch  spreader,   Apply strong & uniform pressure AND press the laminated

 first on the laminate (non porous surface) & then on plywood          portion by using wet squeezed cloth                          or wooden batten or

 (porous surface).                                                     roller  to  remove  air  entraption.                   Sanding  work  can  start


                                                                       after 30 minutes but final bonding is achieved after 24 hrs.









 Give enough open time (10–15 minutes) depending on

 climatic conditions. Ensure touch dry condition before

 pasting laminate. Take care of alignment as there is no

 scope of re-alignment once fixed. Always use a wooden

 log between 2 surfaces for better alignment.









                                                        General Instructions & Precautions for Uses:


 Put a wooden log between the surfaces for              Store awy from direct heat and sunlight

 better alignment and start pasting it from             Skin Formation, If any should be removed before use

 one direction. Take laminate of little bigger          Stir the content of the container well before use


 size (1.5 mm to 2 mm) than ply so that it              Water should not be added for dilution as it

 can be trimmed after pasting.                          may adversely affect the performance of the