6.  From two tests carried out with 2-point load cell on silt sand mixture (50/50) stabilized with
                      cement and ImmoCem it can be concluded that the tensile bending strength of 2.5 to 2.75
                      MPa can be expected and that  the breaking strain at failure of 750 à 875 µm/m can be
                      achieved.
                      This corresponds to the stiffness modulus at failure of  2900 to 3700 MPa.

               As limited as this research is, the results suggest that the ImmoCem material has potentially a wide
               range of applications in construction.
               The challenge of obtaining and maintaining large strain at failure is  to limit the variation in the
               strength while maintaining the increased average strength. Depending on the intended field
               applications the either the fatigue or the tensile bending strength and/or the compressive  strength
               can be most relevant.