Page 219 - Microsoft Word - 2_Inch_Drain_Adapter_PDS_2016_01_05
P. 219

®
                                                                   ®
                                            DURO-LAST  ROCK-PLY  MEMBRANE


            Membrane Attachment:
              Mechanically Fastened – Rock-Ply membrane may be mechanically attached to a variety of roof deck and wall
              materials. An appropriate slip sheet or cover board may be required. Refer to the Roll Good Mechanically
              Fastened Systems Specification for system requirements.
                        ®
              Duro-Bond  System – The Duro-Bond system (induction weld) may be used to attach Rock-Ply membrane.
              Refer to the Duro-Last Duro-Bond System Specification for system requirements.
              Adhered – Rock-Ply membrane may be adhered to a variety of properly prepared roof decks, walls, cover
              boards and insulations. Refer to the Duro-Last Adhered Systems Specification for system requirements.

            Physical Properties:
            Rock-Ply membrane has been subjected to the tests required by ASTM 4434 “Standard Specification for Poly
            (Vinyl Chloride) Sheet Roofing” and has been classified as a Type III, internally reinforced sheet. The results of
            each test are listed below. ASTM’s Overall Thickness requirements for the membrane are plus or minus 10%
            (nominal) of the listed Typical Value.
               Physical Property        Test Method          ASTM D4434 Requirement   Result     Typical Value
                                                                0.045 and ≤ 0.055 in.
               Overall Thickness        ASTM D751                                     PASS   0.050 in. (50 mil), nominal
                                                                ( 45 and ≤ 55 mil)
             Thickness Over Scrim      ASTM D7635                   0.016 in.        PASS      0.021 in. (21 mil)
                            1
              Breaking Strength    ASTM D751 Grab Method            200 lbf./in.     PASS      390 x 438 lbf./in.
                         1
                 Elongation        ASTM D751 Grab Method              15%            PASS        31% x  31%
                                                                     328 lbf.
                Seam Strength      ASTM D751 Grab Method                              PASS         417 lbf.
                                                             (75% of Breaking Strength.)
                          1
                Tear Strength      ASTM D751 Procedure B             45 lbf.         PASS       132 x 163 lbf.
               Low Temp. Bend          ASTM D2136               Must pass at -40 F   PASS          PASS
                                                            Conditioned for 56 days in oven
                 Heat Aging            ASTM D3045                                     PASS          PASS
                                                               maintained at 176 F.
                                                              5,000 hours total test time.
                                        ASTM G154          Irradiance level of 0.68 W/m2-nm.
              Accelerated Aging                                                       PASS          PASS
                                       (Formerly G53)         Cycle: 8 hours at 145 F,
                                                            4 hours condensation at 122 F.
                                                            Conditioned for 6 hours in oven
                             1
             Dimensional Stability     ASTM D1204              maintained at 176 F.   PASS     -0.30% x -0.45%
                                                              Allowable change: ≤ 0.5%
                                                             Immersed in water at 158 F
               Water Absorption         ASTM D570                 for 168 hours.      PASS          1.7%
                                                            Allowable weight change: ≤ 3%
               Static Puncture         ASTM D5602                    33 lbf.         PASS          56 lbf.
              Dynamic Puncture         ASTM D5635                 14.7 ft-lbf. (20 J)   PASS    14.7 ft-lbf. (20 J)
            1
             Typical values are shown for both machine and cross machine directions. The machine direction results are listed first.
            Additional Tests

                   Fungi Resistance              ASTM G-21                  No sustained growth or discoloration
               Moisture Vapor Transmission   ASTM E96, Proc. B, Method A           < 0.35 U.S. perms
















               www.duro-last.com                            2 of 2                             800-248-0280
                                 Duro-Last, “World’s Best Roof”, Rock-Ply and Duro-Bond are registered trademarks owned by Duro-Last, Inc.
                                         Created: 08/01/2008 Revised: 02/25/2013, 07/29/2014, 05/18/2015, 02/15/2016
   214   215   216   217   218   219   220   221   222   223   224