Page 481 - Master Catalog 2017, Inch
P. 481

WMT  Turning, Grooving, Cut-Off, and Profi ling
                                                                              ™
                                                                                           Choosing the Correct WMT Tooling




                      5 Select grade:
                                                                          Recommended Grades
                     Grooving                                                       non-ferrous  high-temp  hardened
                     cutting condition               steel   stainless steel  cast iron  metals  alloys    materials

                     heavily interrupted cut       WU25PT      WU25PT     WU25PT     WU25PT     WU25PT       –



                                                   WP25CT/               WP25CT/
                     lightly interrupted cut                   WU25PT                WU25PT     WU25PT       –
                                                   WU25PT                 WU25PT
                     varying depth of cut, casting,  WU10PT    WU10PT    WP10CT/     WU10PT     WU10HT/    WU10PT
                     or forging skin                                      WU10PT                WU10PT

                                                   WP10CT/               WP10CT/                WU10HT/
                     smooth cut, pre-turned surface            WU10PT                WU10PT                WU10PT
                                                   WU10PT                 WU10PT                WU10PT



                                                                          Recommended Grades
                     Cut-Off                                                        non-ferrous  high-temp  hardened
                     cutting condition               steel   stainless steel  cast iron  metals  alloys    materials
                     heavily interrupted cut       WU25PT      WU25PT     WU25PT     WU25PT     WU25PT       –



                     lightly interrupted cut       WU25PT      WU25PT     WU25PT     WU25PT     WU25PT       –


                     varying depth of cut, casting,  WU25PT    WU25PT     WU25PT     WU25PT     WU25PT     WU25PT
                     or forging skin


                     smooth cut, pre-turned surface  WU25PT    WU25PT     WU25PT     WU25PT     WU25PT     WU25PT

                      NOTE: See page E11 for Grades and Grade Descriptions.


                      6  Determine cutting data:
                        A  Based on material group and grade,
                        identify starting speed (vc).
                      B  First choice starting speed is in bold.


                                                                                          B
                        NOTE: See pages E13–E14 for cutting data.
                                                                 A























                  widia.com                                                                                         E9





         WID_Master16_Turning_Grooving&CutOff_E008_E009_Minch_REBRAND.indd   9                                     11/10/15   11:12 AM
   476   477   478   479   480   481   482   483   484   485   486