Page 101 - final report_Neat
P. 101
• Wire trays wire inserted through the secondary beam . at
first, I thought it might be fault, but structure engineer
guided me that it was possible to do so and was not fault
in constructions.
• The presence of
uneven surface in
the wall require
more thickness of
plaster to achieve
even surface
sometime if
thickness exceed
more than 30mm
then wire mesh are
used
• Wall of 250 thick is
left to place the
concealed cistern
then after
placement finishing
is done with 15
mm of plaster
work
• This id how curing is done in slab
for 5-7 days
• Duct are left for the
transmission of pipe
from floor to floor but
the pies coming out
from basin shower and
wc cannot be
predictable so during
construction void is
created directly below
the slab and are
hidden by false ceiling
80