Page 21 - report P Lemoine feb 2013c
P. 21

21













                                                      crystal region

                                  140
                                  120

                                  100
                                E, GPa  80

                                   60
                                   40
                                   20

                                    0
                                         Y asrec   Y fired    Y N2      Y acid  no Y asrec

               Figure 15: Bar chart of the Young Modulus (E) values for Y as rec, Y fired, Y acid, Y

                                      N2 and no Y as rec on the crystal regions.



                                                       crystal region


                                   25

                                   20


                                  H, GPa  15

                                   10

                                    5


                                    0
                                         Y asrec   Y fired    Y N2      Y acid  no Y asrec


                 Figure 16: Bar chart of the Hardness (H) values for Y as rec, Y fired, Y acid, Y N2
                                       and no Y as rec on the crystal  regions.








                                                                                                        21