SELF-LEVELLING GLAZING LIQUID FILLER  - DIRECTIONS FOR USE



        Professional Liquid Filler
                             Base:
                             The surface must be clean and grease free.



                             Mixing:
                             No more than 2 (by weight) parts of hardener paste should be added to 100 parts of Self-Levelling Glazing
                             Liquid Filler. Excessive amounts of hardener paste can result in peroxide bleaching of the paint. Mix until
                             uniform colour is observed.




             2% hardener

                             Working Time:
                             Working time is the processing time (4-5 minutes) after the Liquid Filler and the Hardener are mixed together.







            4-5 min. 20°C

                             Hardening Time:
                                                                                    o
                             This is the amount of time until the repaired base can receive further work. At 20 C 15–20 minutes is normally required
                             before the filler can be sanded. When temperature is warmer the drying time shortens: If the temperature is cooler the
                             drying time lengthens. To gain time in the drying process, in winter, it is advised that metal surfaces are warmed using
                             infra-red or other heat lamps prior to application.



           15-20 min. 20°C

                             Finishing:
                             The surface must be dry before finishing by sanding or filing. Sand with 40 - 180 grit paper.








              P40 - 180