Page 322 - Wurth Total Catalogue
P. 322
k-plus - DirEctioNs For usE
Professional Body Filler
Base:
he surface must be clean and grease free. o achieve good adhesion be sure that the surface is rough. o not use this product over a thermoplastic acrylic
system (acrylic or lacquer primer surfaces).
Mixing:
o more than 2 by weight parts of hardener paste should be added to 100 parts of lus filler. Excessive
amounts of hardener paste can result in peroxide bleaching of the paint. ix until uniform colour is observed.
2% hardener
Working Time:
or ing time is the processing time minutes after the filler and the Hardener are mixed together.
4-5 min. 20°C
Hardening Time:
o
This is the amount of time until the repaired base can receive further work. At 20 C 15–20 minutes is normally required
before the filler can be sanded. hen temperature is warmer the drying time shortens: f the temperature is cooler the
drying time lengthens. o gain time in the drying process, in winter, it is advised that metal surfaces are warmed using
infra-red or other heat lamps prior to application.
15-20 min. 20°C
Finishing:
he surface must be dry before finishing by sanding or filing. Sand with 0 1 0 grit paper.