               Clinical Pharmacy-Pharm D        Level Three        2  Semester       2024/2025      Pharmaceutical Technology (PT 607)


                                 Causes                                     Remedies

                           Inefficient drying.                 Use efficient and optimum drying
                                                                            conditions.
                 Higher rate of application of coating  Increase viscosity of coating solution
                                 solution.                     to decrease spray application rate


                 3-  Blooming
               It is defect where coating becomes dull immediately or after prolonged storage
               at high temperatures.












                                 Causes                                     Remedies

                 High      concentration      and     low  Decrease  plasticizer  concentration
                 molecular weight of plasticizer used  and  increase  molecular  weight  of
                 in the coating solution.                    plasticizer.



                 4-  Blushing:
               It is a defect best described as whitish specks or haziness in the film.











                                 Causes                                     Remedies


                 High coating temperature.                   Decrease the drying air temperature.

                 Use of sorbitol in formulation which  Avoid use of sorbitol with
                 causes  rapid  precipitation  of  the  Hydroxy  Propyl  Cellulose,  Hydroxy
                 Hydroxy  Propyl  Cellulose,  hydroxy  Propyl  Methyl  Cellulose,  Methyl
                 Propyl  Methyl  Cellulose,  Methyl  Cellulose and Cellulose ethers.